HDPE injection grades by melt flow: J2200, JG910, M80063S, J2210, 17450N, HI1600
For injection HDPE, melt flow largely decides the application: low MFR for impact-resistant crates and pails, high MFR for caps and thin-walled containers. The table orders six grades from low to high MFR.
Updated: 17 Nov 2026 · Thien An Plastics
TDS comparison
| Property | J2200 Lotte Chemical (Hivorex) | JG910 SK Geo Centric (Yuclair) | M80063S SABIC | J2210 Uz-Kor Gas Chemical | 17450N Dow | HI1600 Lotte Chemical |
|---|---|---|---|---|---|---|
| Melt flow (190 °C/2.16 kg) | 5 g/10 min | 5 g/10 min | 8 g/10 min | 7.0–8.0 g/10 min | 17 g/10 min | 20 g/10 min |
| Density | 0.965 g/cm³ | 0.963 g/cm³ | 0.964 g/cm³ | 0.958–0.962 g/cm³ | 0.95 g/cm³ | 0.957 g/cm³ |
| Tensile strength at yield | 25.5 MPa | 260 kg/cm² (≈25.5 MPa) | 25 MPa | ≥ 220 kg/cm² | 22.8 MPa | 280 kg/cm² (≈27.5 MPa) |
| Flexural modulus | 1373 MPa | — | 864 MPa | ≥ 11000 kg/cm² | — | — |
| Notched Izod impact (23 °C) | 98 J/m | 10 kg·cm/cm (≈98.1 J/m) | 84 J/m | — | — | 2 kg·cm/cm (≈19.6 J/m) |
| Vicat softening point | 124 °C | 124 °C | 128 °C | ≥ 122 °C | — | 122 °C |
| Elongation at break | — | — | — | — | 300 % | — |
| ESCR | — | — | — | — | 3 h | — |
| Shore D hardness | — | — | — | — | — | 65 |
Typical values from each producer's TDS, for reference only, not guaranteed specifications. "—" means not stated on the TDS. Values marked "≈" are unit conversions by Thien An for easier comparison.
Key differences
- MFR 5: J2200 (Lotte) and JG910 (SK) are almost equivalent – tensile ≈25.5 MPa, Izod ≈98 J/m, Vicat 124 °C.
- MFR 7–8: M80063S (SABIC) is UV-stabilised per its producer – suited to outdoor products; J2210 (Uz-Kor) reports its specs as ranges.
- MFR 17–20: 17450N (Dow) and HI1600 (Lotte) flow easily into thin walls but have much lower impact (HI1600 ≈20 J/m); 17450N reports ESCR 3 h.
- Higher MFR eases molding but usually lowers impact toughness and stress-crack resistance.
Which grade to choose?
- Crates, pails, pallets needing impact strength: J2200 or JG910.
- Outdoor products: M80063S.
- Caps, containers, thin-walled housewares: 17450N or HI1600.
Tips when switching grades
- Compare like with like: same test method and units (ISO/ASTM; MPa or kg/cm²; Izod or Charpy). Values from different methods are not directly comparable.
- Melt flow has a lot-to-lot tolerance – check the COA of the actual lot, not just the TDS.
- Different additives (nucleating, antistatic, antioxidant, slip) can change the part even when key values match.
- Always trial on your own machine and mold: check temperature, pressure, shrinkage, colour and appearance before switching volume.
FAQ
Can J2200 and JG910 replace each other?
Per TDS both are MFR 5 with almost equal tensile and impact, so usually yes; still trial for shrinkage and colour.
Why does high-MFR HDPE crack more easily?
Higher MFR means shorter molecules – easier filling but lower impact and stress-crack resistance.
Do outdoor parts need UV-stabilised HDPE?
Use a UV-stabilised grade (such as M80063S) or add a UV masterbatch to limit embrittlement and fading in sunlight.
Grade pages with TDS downloads: J2200 · JG910 · M80063S · J2210 · 17450N · HI1600
Other comparisons: LDPE film grades · LLDPE film grades · HDPE film grades · HDPE pipe grades · HDPE for large blow-molded parts · HDPE for monofilament, nets and tape
Based on producers' public TDS, for technical reference only. For grade advice or a quote, contact Thien An Plastics: +84 389 980 742 (WhatsApp, WeChat, Zalo).