HDPE for monofilament, nets and tape: H5480S vs HD53EA010 vs GF7750M2
Fishing nets, rope, woven-sack tape and tarpaulin use fiber-grade HDPE with melt flow around 1. The three grades below share that range but are aimed at slightly different products.
Updated: 17 Nov 2026 · Thien An Plastics
TDS comparison
| Property | H5480S SCG Chemicals | HD53EA010 Reliance Industries | GF7750M2 LyondellBasell |
|---|---|---|---|
| Melt flow (190 °C/2.16 kg) | 0.8 g/10 min | 1 g/10 min | 1 g/10 min |
| Density | 0.952 g/cm³ | 0.955 g/cm³ | 0.957 g/cm³ |
| Melting point | 131 °C | — | 135 °C |
| Vicat softening point | 126 °C | 127 °C | — |
| Tensile strength at yield | 270 kg/cm² (≈26.5 MPa) | 23 MPa | — |
| Elongation at break | 1200 % | — | — |
| Notched Izod impact (23 °C) | 167 J/m | — | — |
| ESCR | 30 h | — | — |
| Flexural modulus | — | 820 MPa | — |
| Melt flow (190 °C/5 kg) | — | — | 3.3 g/10 min |
| Melt flow (190 °C/21.6 kg) | — | — | 33 g/10 min |
Typical values from each producer's TDS, for reference only, not guaranteed specifications. "—" means not stated on the TDS. Values marked "≈" are unit conversions by Thien An for easier comparison.
Key differences
- H5480S (SCG) reports the most data: MFR 0.8, 1,200 % elongation, 167 J/m Izod, ESCR 30 h – for both monofilament and tape.
- HD53EA010 (Reliance) has MFR 1 and 820 MPa flexural modulus, aimed at tape.
- GF7750M2 (LyondellBasell) has MFR 1 and melting point 135 °C, aimed at monofilament and netting.
- Producers report different properties, so actual yarn strength needs a trial on your line.
Which grade to choose?
- Plants making both nets and tape: H5480S.
- Tape for woven sacks and tarpaulin: HD53EA010.
- Monofilament, nets, rope: GF7750M2 or H5480S.
Tips when switching grades
- Compare like with like: same test method and units (ISO/ASTM; MPa or kg/cm²; Izod or Charpy). Values from different methods are not directly comparable.
- Melt flow has a lot-to-lot tolerance – check the COA of the actual lot, not just the TDS.
- Different additives (nucleating, antistatic, antioxidant, slip) can change the part even when key values match.
- Always trial on your own machine and mold: check temperature, pressure, shrinkage, colour and appearance before switching volume.
FAQ
What MFR suits HDPE fiber?
Usually around 0.7–1 g/10 min (190 °C/2.16 kg). Lower MFR gives stronger yarn, higher MFR draws more easily at higher speed.
Can H5480S replace HD53EA010?
Both are in the same MFR range and suit tape, so yes after a trial to adjust draw ratio and temperature.
HDPE or PP for woven sacks?
Woven sacks mostly use PP raffia; HDPE is used for tarpaulin, nets and products needing flexibility and toughness at low temperature.
Grade pages with TDS downloads: H5480S · HD53EA010 · GF7750M2
Other comparisons: LDPE film grades · LLDPE film grades · HDPE film grades · HDPE injection grades by melt flow · HDPE pipe grades · HDPE for large blow-molded parts
Based on producers' public TDS, for technical reference only. For grade advice or a quote, contact Thien An Plastics: +84 389 980 742 (WhatsApp, WeChat, Zalo).