TDS comparison
| Property | FS253S Sumitomo Chemical | HB18N QAMAR | HP1018BN LG Chem | LLD7050 Yulong Petrochemical |
|---|---|---|---|---|
| Melt flow (190 °C/2.16 kg) | 2.2 g/10 min | 0.5 g/10 min | 1 g/10 min | 2 g/10 min |
| Density | 0.922 g/cm³ | 0.918 g/cm³ | 0.918 g/cm³ | 0.919 g/cm³ |
| Melting point | 122 °C | 122 °C | 118 °C | — |
| Dart impact | 90 g | 130 g | 700 g | 55 g |
| Haze | 15 % | 7 % | 18 % | 18 % |
| Vicat softening point | — | 102 °C | — | — |
| Elongation at break | — | — | — | 400 % |
Typical values from each producer's TDS, for reference only, not guaranteed specifications. "—" means not stated on the TDS. Values marked "≈" are unit conversions by Thien An for easier comparison.
Key differences
- HP1018BN is LG Chem metallocene LLDPE with 700 g dart – far above the 55–130 g of the other three.
- HB18N has low MFR (0.5) and 130 g dart, additive-free – suited to thick, heavy-duty film.
- FS253S (MFR 2.2) is general-purpose; LLD7050 (MFR 2) contains slip and antiblock, dart 55 g.
- Dart depends strongly on test film thickness; producers may test at different gauges, so compare only under the same conditions.
Which grade to choose?
- High puncture resistance, thin but strong film: HP1018BN (often blended with LDPE or other LLDPE).
- Thick heavy-duty film and sacks: HB18N.
- General bags and film: FS253S.
- Film needing slip and anti-blocking: LLD7050.
Tips when switching grades
- Compare like with like: same test method and units (ISO/ASTM; MPa or kg/cm²; Izod or Charpy). Values from different methods are not directly comparable.
- Melt flow has a lot-to-lot tolerance – check the COA of the actual lot, not just the TDS.
- Different additives (nucleating, antistatic, antioxidant, slip) can change the part even when key values match.
- Always trial on your own machine and mold: check temperature, pressure, shrinkage, colour and appearance before switching volume.
FAQ
How does mLLDPE differ from regular LLDPE?
mLLDPE uses metallocene catalyst, giving narrow molecular weight distribution and much tougher, more puncture-resistant film (HP1018BN dart 700 g), but it is often harder to process and usually blended with LDPE.
Can HB18N (MFR 0.5) make thin film?
Low MFR flows less, so it suits thick, heavy-duty film. For thin film, blend with a higher-flow grade or LDPE and trial first.
Is higher dart always better?
Higher dart means better puncture resistance, but clarity, stiffness, sealing and price also matter. Choose by product needs.
Grade pages with TDS downloads: FS253S · HB18N · HP1018BN · LLD7050
Other comparisons: LDPE film grades · HDPE film grades · HDPE injection grades by melt flow · HDPE pipe grades · HDPE for large blow-molded parts · HDPE for monofilament, nets and tape