PP for spunbond nonwovens: Y-26, Y-35, UH563S, HP565S, S2040 and Y40L compared
Spunbond nonwoven uses PP homopolymer with melt flow around 25–40. The seven grades below are all in this range and differ mainly in MFR and how much detail their TDS gives.
Updated: 17 Nov 2026 · Thien An Plastics
TDS comparison
| Property | Y-26 Luqing Petrochemical | Y-35 Luqing Petrochemical | UH563S Polymirae (UlsanPP) | HP565S LyondellBasell | S2040 (Shenhua) Shenhua (CHN Energy) | S2040 Oriental Energy | Y40L Dongguan |
|---|---|---|---|---|---|---|---|
| Melt flow (230 °C/2.16 kg) | 26 g/10 min | 35 g/10 min | 38 g/10 min | 38 g/10 min | 38 ± 7 g/10 min | 40 g/10 min | 40 g/10 min |
| Tensile strength at yield | 31.6 MPa | 31.7 MPa | — | — | ≥ 31.0 MPa | — | 29 MPa |
| Density | — | — | 0.9 g/cm³ | — | — | — | — |
| Vicat softening point | — | — | 153 °C | — | — | — | — |
| Isotacticity | — | — | — | — | ≥ 95 % | — | — |
| Ash content | — | — | — | — | ≤ 300 mg/kg | — | — |
| Yellow index | — | — | — | — | ≤ 4.0 | — | — |
Typical values from each producer's TDS, for reference only, not guaranteed specifications. "—" means not stated on the TDS. Values marked "≈" are unit conversions by Thien An for easier comparison.
Key differences
- MFR ranges from 26 (Y-26) to 40 (S2040, Y40L). Lower MFR usually gives coarser fibre and stronger fabric; higher MFR spins finer fibre, softer fabric and faster lines.
- UH563S, HP565S and S2040 Shenhua all have MFR 38 – the most interchangeable group.
- S2040 Shenhua and Y40L also state quality specs: isotacticity ≥95 %, ash and yellow index – useful for white hygiene and medical fabric.
- Many TDS list only MFR, so trial on the spunbond line when switching grades.
Which grade to choose?
- Strong, heavier fabric: Y-26, Y-35.
- General fabric with flexible sourcing: the MFR 38 group (UH563S, HP565S, S2040 Shenhua).
- Soft, light fabric for diapers and masks: S2040, Y40L.
Tips when switching grades
- Compare like with like: same test method and units (ISO/ASTM; MPa or kg/cm²; Izod or Charpy). Values from different methods are not directly comparable.
- Melt flow has a lot-to-lot tolerance – check the COA of the actual lot, not just the TDS.
- Different additives (nucleating, antistatic, antioxidant, slip) can change the part even when key values match.
- Always trial on your own machine and mold: check temperature, pressure, shrinkage, colour and appearance before switching volume.
FAQ
What MFR suits spunbond PP?
Typically about 25–40 g/10 min (230 °C/2.16 kg), chosen by fibre fineness, fabric weight and line speed.
Can UH563S, HP565S and S2040 replace each other?
All have MFR 38, so usually yes, but trial because spinning stability also depends on additives and molecular weight distribution.
Can spunbond PP make the mask filter layer?
No. The middle filter layer is meltblown fabric using very high-flow PP; spunbond PP is for the outer and inner layers.
Grade pages with TDS downloads: Y-26 · Y-35 · UH563S · HP565S · S2040 (Shenhua) · S2040 · Y40L
Other comparisons: LDPE film grades · LLDPE film grades · HDPE film grades · HDPE injection grades by melt flow · HDPE pipe grades · HDPE for large blow-molded parts
Based on producers' public TDS, for technical reference only. For grade advice or a quote, contact Thien An Plastics: +84 389 980 742 (WhatsApp, WeChat, Zalo).