SAN resin (styrene acrylonitrile): INP576 (SAN 576), PN-127 and SAN 350HW compared
SAN (styrene acrylonitrile) is a clear resin that is stiffer, more chemical resistant and more heat resistant than GPPS – used for lighter bodies, fan blades, containers, clear housewares and as a base for ABS compounding. This article compares SABIC’s INP576 (SAN 576), Chi Mei’s PN-127 and Kumho’s SAN 350HW from their TDS.
Updated: 26 November 2026 · Thien An Plastics
Properties from the TDS
| Property | INP576 / SAN 576 SABIC | PN-127 Chi Mei (Taiwan) | SAN 350HW Kumho Petrochemical (Korea) |
|---|---|---|---|
| Melt flow | 23 g/10 min (230 °C/3.8 kg) | MVR 17 ml/10 min (220 °C/10 kg) | 6.0 g/10 min (230 °C/3.8 kg); 1.4 (200 °C/5 kg) |
| Density | 1.08 g/cm³ | 1.06 g/cm³ | 1.07 g/cm³ |
| Tensile strength | 68 MPa (break) | 74 MPa | 810 kg/cm² (≈79.4 MPa) |
| Elongation | 2.2 % (break) | 3 % | 4.5 % |
| Flexural modulus | 3,570 MPa (ASTM D790) | 3.3 GPa (ISO 178) | 35,900 kg/cm² (≈3,521 MPa) |
| Notched Izod impact (23 °C) | 21 J/m | 3 kJ/m² (ISO 180/1A) | 1.5 kg·cm/cm (≈14.7 J/m) |
| HDT (1.8 MPa) | 87 °C (unannealed) | 90 °C (unannealed); 101 °C (annealed) | 94 °C |
| Vicat softening point | 102 °C (B/50) | 105 °C (1 kg); 104 °C (5 kg) | 109 °C (1 kg) |
| Mould shrinkage | — | 0.2–0.7 % | 0.2–0.6 % |
Typical values from each producer's TDS, for reference only and not specifications. "—" means not published in the TDS. Values marked "≈" were converted by Thien An for easier comparison.
Key differences
- Flow: INP576 flows much more under the same condition (23 g/10 min at 230 °C/3.8 kg) than SAN 350HW (6.0) – SABIC calls INP576 a medium-flow SAN. PN-127 is tested to ISO at 220 °C/10 kg, so it is not directly comparable.
- Strength and heat: Kumho describes SAN 350HW as super high strength and high heat – tensile ≈79.4 MPa, HDT 94 °C, Vicat 109 °C, the highest in the group.
- Stiffness: all three have flexural modulus 3.3–3.57 GPa – clearly stiffer than GPPS (~3.1 GPa) and HIPS.
- Applications per TDS: SAN 350HW – disposable lighters, electric fans, electronic parts; PN-127 – general injection, HB at 1.5 mm.
Which grade to choose?
Notes when switching grades
- SAN is brittle (elongation 2–5 %, low impact) – consider ABS for impact-loaded parts.
- SAN absorbs some moisture (SAN 350HW TDS: water absorption 0.3 %): dry before moulding to avoid silver streaks.
- Moulding temperature per the SAN 350HW TDS: nozzle 190–220 °C.
- When moving from low-flow SAN 350HW to higher-flow INP576, reduce melt temperature and injection pressure.
FAQ
How does SAN differ from GPPS?
Both are clear, but SAN contains acrylonitrile, making it stiffer and more chemical and heat resistant; e.g. SAN 350HW has a Vicat of 109 °C vs 95 °C for GP525N per the TDS.
Are INP576 and SAN 576 the same grade?
Both are SABIC Cycolac INP576 (medium-flow SAN); Thien An has two pages based on the Europe and Americas TDS, with the same data.
Which SAN is strongest?
SAN 350HW (Kumho) – tensile 810 kg/cm² (≈79.4 MPa), HDT 94 °C per the TDS.
Where can I buy INP576, PN-127, SAN 350HW with a TDS?
Thien An Plastics supplies INP576, PN-127, SAN 350HW with TDS; contact +84 389 980 742 (WhatsApp, WeChat, Zalo) for a quote.
Grade pages (TDS download): INP576 · SAN 576 · PN-127 · SAN 350HW
More articles: GPPS (crystal PS): GP150, GP525N, 500W, 525B and GPPS 535 compared · ABS D-150 vs DG417 · PMMA (acrylic): ACRYREX CM-205 vs CM-207 compared
Based on producers' public TDS; for technical reference only. For grade advice or a quote, contact Thien An Plastics: +84 389 980 742 (WhatsApp, WeChat, Zalo).