PE for extrusion coating (paper, tarpaulin, woven, laminates): 7019EC, L705, LD 251, LDC801YY and 9730 compared
Paper cups, coated kraft, HDPE tarpaulin, coated woven bags and multi-layer laminates all need a PE layer extruded directly onto the substrate – extrusion coating. Compared with PP coating, PE coating melts lower and heat-seals easily. This article compares 7019EC, L705, LD 251, LDC801YY and 9730 from their TDS.
Updated: 26 November 2026 · Thien An Plastics
Properties from the TDS
| Property | 7019EC SABIC | L705 Sumitomo / Petro Rabigh (Saudi Arabia) | LD 251 ExxonMobil | LDC801YY Lotte Chemical Titan (Malaysia) | 9730 Hanwha TotalEnergies (Korea) |
|---|---|---|---|---|---|
| Melt index (190 °C/2.16 kg) | 7.0 g/10 min | 7 g/10 min | 8.0 g/10 min | 7 g/10 min | 15.0 g/10 min |
| Density | 919 kg/m³ | 0.919 g/cm³ | 0.916 g/cm³ | 0.920 g/cm³ | 0.922 g/cm³ |
| Tensile strength at break | 14 MPa | 14 MPa | — | — | 170 kg/cm² (≈16.7 MPa) |
| Elongation at break | 550 % | 550 % | — | — | 670 % |
| Vicat softening point | 86 °C | 86 °C | — | 86 °C | 94 °C |
| Melting point | 106 °C | 106 °C | 104 °C (peak) | — | — |
| Neck-in | — | — | 4.0 cm (50 m/min); 3.8 cm (100 m/min), 315 °C | 9 cm (50 m/min, 295 °C) | 4.5 cm (100 m/min, 305 °C) |
| Moisture vapour transmission | — | — | — | 18.5 g/m²/24h (25 µm, 37.8 °C, 90 % RH) | 7.0 g/m²/24h (ASTM F1249) |
| Processing temperature (TDS) | 300–340 °C | 280–340 °C | — | 270–340 °C | cylinder 200–300 °C; die 300 °C |
| Additives | No slip / anti-block | No stabiliser, slip, anti-block | No slip, anti-block, stabiliser | Barefoot (none) | Antioxidant |
Typical values from each producer's TDS, for reference only and not specifications. "—" means not published in the TDS. Values marked "≈" were converted by Thien An for easier comparison.
Key differences
- High-pressure LDPE, MI 7–8: 7019EC, L705, LD 251 and LDC801YY are standard LDPE coating grades without slip/anti-block. 7019EC and L705 have almost identical data (MI 7, density 0.919, Vicat 86 °C, melting 106 °C).
- 9730 is different: made by the UNIPOL gas-phase process with MI 15 – high flow; Hanwha cites excellent draw-down, low neck-in (4.5 cm), strong adhesion to HDPE yarn and PP woven cloth and coating speed >500 m/min; mainly for tarpaulin. Highest Vicat (94 °C).
- Neck-in: LD 251 lists low neck-in (3.8–4.0 cm), good heat sealing at high speed and low odour/taste; LDC801YY lists 9 cm under its own conditions – not directly comparable.
- Applications per TDS: L705 – coating OPA/OPP film, kraft paper, aluminium, PE woven cloth; LD 251 – co-extrusion coating, extrusion lamination, nonwoven coating, food and liquid packaging, photographic paper; LDC801YY – coating all substrates, excellent draw-down, good heat sealability and adhesion.
Which grade to choose?
Notes when switching grades
- Switching between MI 7–8 and MI 15 (9730) changes neck-in and edge bead – re-adjust air gap, temperature and line speed.
- PE coating runs very hot (270–340 °C): check odour and fumes, especially for food packaging.
- Each producer measures neck-in under its own conditions – trial on the real line.
- LD 251 is the new name of ExxonMobil LD 8016.BA (the TDS on the site shows the old name).
- See also PP extrusion coating.
FAQ
How does PE coating differ from PP coating?
PE coating (MI 7–15 at 190 °C) melts at about 104–106 °C and heat-seals easily – for paper, liquid packaging and laminates; PP coating (MFR 24–30 at 230 °C) melts at 136–162 °C, is stiffer and is widely used for woven bags.
Which grade is for HDPE tarpaulin?
9730 (Hanwha TotalEnergies) – the TDS states it is designed especially for tarpaulin, with strong adhesion to HDPE yarn and PP woven cloth.
Is LD 251 the same as LD 8016.BA?
Yes, LD 251 is the new name of ExxonMobil LD 8016.BA.
Where can I buy 7019EC, L705, LD 251, LDC801YY, 9730 with a TDS?
Thien An Plastics supplies 7019EC, L705, LD 251, LDC801YY, 9730 with TDS; contact +84 389 980 742 (WhatsApp, WeChat, Zalo) for a quote.
Grade pages (TDS download): 7019EC · L705 · LD 251 · LDC801YY · 9730
More articles: PP for extrusion coating (woven bags, kraft paper, BOPP): 3375RM, F801C, L-270A, P838C and FC9415P compared · LDPE film: FD0270, FD0274, FD0474, 4025AS · PP for CPP cast film: 1102M, HP2100L, H4540, UH513M and SFC-550 compared