NHỰA THIÊN ANTHIEN AN PLASTICS Request a quote
Knowledge · Grade comparison

LLDPE for cast stretch film: 2607G, GA1820, 222NJ, 318BJ, HF1820, HF1832 and XP9400 compared

Pallet stretch film is mostly made on multilayer cast lines and needs resins that run stably at high speed, stretch deeply without breaking and hold the load well. The seven LLDPE grades below all have density around 0.915–0.921 g/cm³ and MI 2–3.7, but differ in comonomer and toughness.

Updated: 22 November 2026 · Thien An Plastics

Properties from the TDS

Property2607G
Dow
GA1820
LyondellBasell
222NJ
SABIC
318BJ
SABIC
HF1820
Sasol
HF1832
Sasol
XP9400
Daelim / DL Chemical (Korea)
Type / comonomer (per TDS)———ButeneHexeneHexenemLLDPE (metallocene)
Melt index (190 °C/2.16 kg)2.3 g/10 min2.0 g/10 min2.2 g/10 min2.8 g/10 min2.0 g/10 min3.2 g/10 min3.7 g/10 min
Density0.918 g/cm³0.918 g/cm³0.921 g/cm³0.918 g/cm³0.918 g/cm³0.918 g/cm³0.915 g/cm³
Test film thickness (cast)23 µm20.3 µm20 µm20 µm20 µm25.4 µm22 µm
Tensile strength at break MD/TD35 / 29 MPa35 / 22 MPa40 / 30 MPa—55.7 / 47.2 MPa—620 / 560 kg/cm² (≈60.8 / 54.9 MPa)
Elongation at break MD/TD460 / 700 %380 / 720 %670 / 850 %—480 / 890 %750 / 830 %545 / 660 %
Dart impact150 g (ISO 7765-1/A)90 g (F50)65 g2.6 kJ/m (ISO 7765-2)165 g/mil (F50)120 g550 g (A)
Elmendorf tear MD/TD190 / 420 g430 / 840 g70 / 215 gTD 140 kN/m (ISO 6383-2)280 / 813 g/mil370 / 500 g—
Haze—2 %0.7 %2.1 % (30 µm)2.5 %2.5 %0.3 %

Typical values from each producer's TDS, for reference only and not specifications. "—" means not published in the TDS. Values marked "≈" were converted by Thien An for easier comparison.

Key differences

Note: dart and tear are measured with different methods and gauges (g, g/mil, kJ/m, kN/m); compare only within the same method.

Which grade to choose?

Notes when switching grades

FAQ

Which LLDPE is best for pallet stretch film?

It depends on the line and requirement: 2607G as core layer on large lines; GA1820 or HF1820 for tough film; HF1832 or XP9400 for thin, deep-stretch film. Trial on your own line.

How does hexene LLDPE differ from butene?

Per the TDS, hexene grades (HF1820, HF1832) show higher tensile strength and film toughness than butene grades such as 318BJ.

Can XP9400 be used for food wrap?

The XP9400 TDS lists food packaging wrap and compliance with FDA 21 CFR 177.1520 and EU 10/2011. The final product must still be assessed against the target market’s rules.

Is the TDS available?

Yes. Each grade page on thienanplastics.com has the TDS for download.

Grade pages (TDS download): DOWLEX 2607G · GA1820 · 222NJ · 318BJ · HF1820 · HF1832 · XP9400

More articles: Metallocene mLLDPE film grades: HP1018BN, D139FK, XP9200 and HPR3518CB compared · LLDPE film grades: FS253S, HB18N, HP1018BN, LLD7050 · LLDPE injection moulding grades: UI2420, UI2650, UL814, DNDA-8320, LL 6100, LL 6201.19, M200024 and HM2420

Based on producers' public TDS; for technical reference only. For grade advice or a quote, contact Thien An Plastics: +84 389 980 742 (WhatsApp, WeChat, Zalo).

Zalo